{"id":4184,"date":"2026-04-16T08:27:58","date_gmt":"2026-04-16T06:27:58","guid":{"rendered":"https:\/\/shockwave-clad.com\/explosion-bonding\/"},"modified":"2026-10-22T13:39:00","modified_gmt":"2026-10-22T11:39:00","slug":"soldadura-por-explosion","status":"publish","type":"page","link":"https:\/\/shockwave-clad.com\/es\/soldadura-por-explosion\/","title":{"rendered":"Soldadura por explosi\u00f3n"},"content":{"rendered":"<p>[et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.4&#8243; background_color=\u00bb#000000&#8243; background_image=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2025\/09\/electrician_19.png\u00bb background_position=\u00bbtop_center\u00bb custom_padding=\u00bb54px|0px|0|0px|false|false\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row _builder_version=\u00bb4.27.5&#8243; global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb4_4&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb header_font=\u00bbGoldman Sans|300|||||||\u00bb header_text_color=\u00bb#FFFFFF\u00bb header_font_size=\u00bb48px\u00bb custom_margin=\u00bb||0px||false|false\u00bb custom_padding=\u00bb||0px||false|false\u00bb header_font_size_tablet=\u00bb42px\u00bb header_font_size_phone=\u00bb32px\u00bb header_font_size_last_edited=\u00bbon|phone\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h1><strong>Soldadura por explosi\u00f3n: proceso, aplicaciones y ventajas<\/strong><\/h1>\n<p>[\/et_pb_text][et_pb_text _builder_version=\u00bb4.27.4&#8243; text_font=\u00bb||||||||\u00bb header_6_font=\u00bbGoldman Sans|600|||||||\u00bb header_6_text_color=\u00bb#FFFFFF\u00bb header_6_font_size=\u00bb18px\u00bb header_6_line_height=\u00bb1.8em\u00bb max_width=\u00bb60px\u00bb height=\u00bb0px\u00bb custom_margin=\u00bb0px||30px||false|false\u00bb custom_padding=\u00bb0px||0px||false|false\u00bb border_color_all=\u00bb#FFB356&#8243; border_width_bottom=\u00bb2px\u00bb border_color_bottom=\u00bb#ffb356&#8243; locked=\u00bboff\u00bb global_colors_info=\u00bb{}\u00bb][\/et_pb_text][\/et_pb_column][\/et_pb_row][et_pb_row column_structure=\u00bb1_2,1_2&#8243; _builder_version=\u00bb4.27.4&#8243; custom_padding=\u00bb||60px||false|false\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#FFFFFF\u00bb text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb max_width=\u00bb600px\u00bb custom_margin=\u00bb||||false|false\u00bb custom_margin_tablet=\u00bb|||0px\u00bb custom_margin_phone=\u00bb\u00bb custom_margin_last_edited=\u00bbon|desktop\u00bb hover_enabled=\u00bb0&#8243; global_colors_info=\u00bb{}\u00bb sticky_enabled=\u00bb0&#8243;]<\/p>\n<p>La soldadura por explosi\u00f3n (explosion bonding) es un proceso de soldadura en fr\u00edo por presi\u00f3n en estado s\u00f3lido que une metales dis\u00edmiles sin fundirlos. Mediante energ\u00eda explosiva controlada, esta t\u00e9cnica crea una uni\u00f3n at\u00f3mica de alta resistencia entre materiales con propiedades muy diferentes.<\/p>\n<p>Esto permite fabricar placas revestidas (clad plates), placas tubulares y juntas de transici\u00f3n de alto rendimiento para sectores exigentes como el petr\u00f3leo y gas, offshore, energ\u00eda y procesamiento qu\u00edmico.<\/p>\n<p>En Shockwave Metalworking Technologies estamos especializados en la <span style=\"color: #ff9900;\"><a href=\"https:\/\/shockwave-clad.com\/es\/tecnologia\/\" style=\"color: #ff9900;\"><strong>soldadura por explosi\u00f3n al vac\u00edo<\/strong><\/a><\/span>, un proceso avanzado que mejora la calidad de la uni\u00f3n y ofrece soluciones fiables y de alta integridad para entornos cr\u00edticos donde los m\u00e9todos de uni\u00f3n convencionales no son adecuados. Por ello es una de las tecnolog\u00edas m\u00e1s eficaces y vers\u00e1tiles para unir metales dis\u00edmiles en aplicaciones industriales.<\/p>\n<p>[\/et_pb_text][\/et_pb_column][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_image src=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2026\/10\/Introduction-opt.webp\u00bb alt=\u00bbPlacas revestidas fabricadas por soldadura por explosi\u00f3n en Shockwave Metalworking Technologies\u00bb title_text=\u00bbPlacas revestidas fabricadas por soldadura por explosi\u00f3n en Shockwave Metalworking Technologies\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb30px\u00bb box_shadow_vertical=\u00bb30px\u00bb box_shadow_spread=\u00bb10px\u00bb box_shadow_color=\u00bbrgba(255,255,255,0.3)\u00bb global_colors_info=\u00bb{}\u00bb][\/et_pb_image][\/et_pb_column][\/et_pb_row][et_pb_row column_structure=\u00bb1_2,1_2&#8243; custom_padding_last_edited=\u00bbon|tablet\u00bb _builder_version=\u00bb4.27.4&#8243; custom_margin=\u00bb|||\u00bb custom_padding=\u00bb||||false|false\u00bb custom_padding_tablet=\u00bb|||0px\u00bb custom_padding_phone=\u00bb\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_image src=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2026\/10\/What-is-Explosion-Bonding-opt.webp\u00bb alt=\u00bbPlacas revestidas por explosi\u00f3n al vac\u00edo en Shockwave, cargadas en el cami\u00f3n para su env\u00edo\u00bb title_text=\u00bbPlacas revestidas por explosi\u00f3n al vac\u00edo en Shockwave, cargadas en el cami\u00f3n para su env\u00edo\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb-30px\u00bb box_shadow_vertical=\u00bb-30px\u00bb box_shadow_spread=\u00bb10px\u00bb global_colors_info=\u00bb{}\u00bb][\/et_pb_image][\/et_pb_column][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#FFFFFF\u00bb text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb ul_font=\u00bb||||||||\u00bb ul_line_height=\u00bb1.8em\u00bb header_2_font_size=\u00bb39px\u00bb header_3_font=\u00bbGoldman Sans|700|||||||\u00bb header_3_text_color=\u00bb#FFFFFF\u00bb header_3_font_size=\u00bb38px\u00bb header_3_line_height=\u00bb1.4em\u00bb header_3_font_size_tablet=\u00bb\u00bb header_3_font_size_phone=\u00bb32px\u00bb header_3_font_size_last_edited=\u00bbon|phone\u00bb locked=\u00bboff\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><span style=\"color: #ffffff;\"><strong>\u00bfQu\u00e9 es la soldadura por explosi\u00f3n?<\/strong><\/span><\/h2>\n<p>La soldadura por explosi\u00f3n (tambi\u00e9n llamada revestimiento por explosi\u00f3n o explosion cladding) es un proceso en estado s\u00f3lido que une dos metales diferentes mediante energ\u00eda explosiva controlada, sin alterar las propiedades mec\u00e1nicas ni qu\u00edmicas de los materiales.<\/p>\n<p>Durante el proceso, una detonaci\u00f3n controlada genera un impacto a alta velocidad entre los metales y crea una uni\u00f3n metal\u00fargica en la interfaz. Se produce un <strong>efecto de chorro (jetting)<\/strong> que elimina los contaminantes superficiales y permite el contacto directo metal-metal a nivel at\u00f3mico.<\/p>\n<p>El resultado es una <strong>interfaz metal\u00fargica ondulada, <\/strong>caracter\u00edstica de la soldadura por explosi\u00f3n, que proporciona una resistencia de uni\u00f3n excepcional y fiabilidad a largo plazo incluso en condiciones extremas.<\/p>\n<p>Gracias a estas propiedades, el revestimiento por explosi\u00f3n se utiliza ampliamente en industrias donde el rendimiento, la durabilidad y la resistencia a la corrosi\u00f3n son cr\u00edticos.<\/p>\n<p>[\/et_pb_text][\/et_pb_column][\/et_pb_row][et_pb_row _builder_version=\u00bb4.16&#8243; module_alignment=\u00bbright\u00bb custom_padding=\u00bb30px|0px|0|0px|false|false\u00bb locked=\u00bboff\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb4_4&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_button button_url=\u00bb@ET-DC@eyJkeW5hbWljIjp0cnVlLCJjb250ZW50IjoicG9zdF9saW5rX3VybF9wYWdlIiwic2V0dGluZ3MiOnsicG9zdF9pZCI6IjIwIn19@\u00bb button_text=\u00bbCont\u00e1ctenos\u00bb button_alignment=\u00bbright\u00bb _builder_version=\u00bb4.27.4&#8243; _dynamic_attributes=\u00bbbutton_url\u00bb custom_button=\u00bbon\u00bb button_text_size=\u00bb14px\u00bb button_bg_color=\u00bb#ffb356&#8243; button_border_color=\u00bb#000000&#8243; button_border_radius=\u00bb0px\u00bb button_letter_spacing=\u00bb3px\u00bb button_font=\u00bbGoldman Sans|700||on|||||\u00bb button_icon=\u00bb&#x24;||divi||400&#8243; button_on_hover=\u00bboff\u00bb background_layout=\u00bbdark\u00bb custom_margin=\u00bb|||\u00bb custom_padding=\u00bb30px|70px|30px|70px|true|false\u00bb animation_style=\u00bbfold\u00bb animation_direction=\u00bbright\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb-30px\u00bb box_shadow_vertical=\u00bb-30px\u00bb box_shadow_spread=\u00bb-10px\u00bb box_shadow_color=\u00bbrgba(255,179,86,0.4)\u00bb global_colors_info=\u00bb{}\u00bb button_text_size__hover_enabled=\u00bboff\u00bb button_one_text_size__hover_enabled=\u00bboff\u00bb button_two_text_size__hover_enabled=\u00bboff\u00bb button_text_color__hover_enabled=\u00bboff\u00bb button_one_text_color__hover_enabled=\u00bboff\u00bb button_two_text_color__hover_enabled=\u00bboff\u00bb button_border_width__hover_enabled=\u00bboff\u00bb button_one_border_width__hover_enabled=\u00bboff\u00bb button_two_border_width__hover_enabled=\u00bboff\u00bb button_border_color__hover_enabled=\u00bboff\u00bb button_one_border_color__hover_enabled=\u00bboff\u00bb button_two_border_color__hover_enabled=\u00bboff\u00bb button_border_radius__hover_enabled=\u00bboff\u00bb button_one_border_radius__hover_enabled=\u00bboff\u00bb button_two_border_radius__hover_enabled=\u00bboff\u00bb button_letter_spacing__hover_enabled=\u00bboff\u00bb button_one_letter_spacing__hover_enabled=\u00bboff\u00bb button_two_letter_spacing__hover_enabled=\u00bboff\u00bb button_bg_color__hover_enabled=\u00bboff\u00bb button_one_bg_color__hover_enabled=\u00bboff\u00bb button_two_bg_color__hover_enabled=\u00bboff\u00bb][\/et_pb_button][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.6&#8243; background_enable_color=\u00bboff\u00bb background_enable_image=\u00bboff\u00bb background_position=\u00bbtop_center\u00bb custom_padding=\u00bb54px|0px|0|0px|false|false\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row column_structure=\u00bb1_2,1_2&#8243; _builder_version=\u00bb4.27.4&#8243; custom_padding=\u00bb||22px|0px|false|false\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#FFFFFF\u00bb text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb link_font=\u00bb||||on|||#de8d02|\u00bb link_text_color=\u00bb#de8d02&#8243; ul_text_color=\u00bb#000000&#8243; header_2_font_size=\u00bb39px\u00bb max_width=\u00bb600px\u00bb custom_margin=\u00bb||||false|false\u00bb custom_margin_tablet=\u00bb|||0px\u00bb custom_margin_phone=\u00bb\u00bb custom_margin_last_edited=\u00bbon|desktop\u00bb custom_padding=\u00bb||0px|||\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><span style=\"color: #000000;\"><strong>C\u00f3mo funciona la soldadura por explosi\u00f3n<\/strong><\/span><\/h2>\n<p><span style=\"color: #000000;\">El proceso comienza colocando dos placas met\u00e1licas a una distancia de separaci\u00f3n controlada. A continuaci\u00f3n se detona una carga explosiva que genera un impacto a alta velocidad entre los materiales.<\/span><\/p>\n<p><span style=\"color: #000000;\">A medida que avanza la detonaci\u00f3n, una placa es proyectada contra la otra a gran velocidad. Este impacto crea una uni\u00f3n por deformaci\u00f3n pl\u00e1stica en la interfaz, obteniendo una conexi\u00f3n resistente y continua.<\/span><\/p>\n<p><span style=\"color: #000000;\">Caracter\u00edsticas clave del proceso:<\/span><\/p>\n<ul>\n<li><span style=\"color: #000000;\">Sin fusi\u00f3n de los materiales<\/span><\/li>\n<li><span style=\"color: #000000;\">Zona afectada t\u00e9rmicamente m\u00ednima<\/span><\/li>\n<li><span style=\"color: #000000;\">Uni\u00f3n metal\u00fargica resistente<\/span><\/li>\n<li><span style=\"color: #000000;\">Capacidad de unir metales incompatibles<\/span><\/li>\n<li><span style=\"color: #000000;\">Uni\u00f3n de grandes superficies<\/span><\/li>\n<\/ul>\n<p><span style=\"color: #000000;\">En Shockwave aplicamos esta tecnolog\u00eda mediante la <a href=\"https:\/\/shockwave-clad.com\/es\/tecnologia\/\"><strong>soldadura por explosi\u00f3n al vac\u00edo<\/strong><\/a>, que ofrece un mayor control, reduce la oxidaci\u00f3n y garantiza una uni\u00f3n m\u00e1s homog\u00e9nea.<\/span><\/p>\n<p>[\/et_pb_text][\/et_pb_column][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_image src=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2026\/10\/Vacuum-explosion-bonding-henhanced-Process-Control-opt.webp\u00bb alt=\u00bbSoldadura por explosi\u00f3n al vac\u00edo: control de proceso mejorado\u00bb title_text=\u00bbSoldadura por explosi\u00f3n al vac\u00edo: control de proceso mejorado\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb custom_margin=\u00bb30px|||||\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb30px\u00bb box_shadow_vertical=\u00bb30px\u00bb box_shadow_spread=\u00bb10px\u00bb global_colors_info=\u00bb{}\u00bb][\/et_pb_image][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.4&#8243; background_color=\u00bb#000000&#8243; background_image=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2025\/09\/electrician_19.png\u00bb background_position=\u00bbtop_center\u00bb custom_padding=\u00bb54px|0px|0|0px|false|false\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row column_structure=\u00bb1_2,1_2&#8243; custom_padding_last_edited=\u00bbon|tablet\u00bb _builder_version=\u00bb4.27.4&#8243; min_height=\u00bb682.1px\u00bb custom_margin=\u00bb|auto|-50px|auto||\u00bb custom_padding=\u00bb||||false|false\u00bb custom_padding_tablet=\u00bb|||0px\u00bb custom_padding_phone=\u00bb\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_image src=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2026\/10\/Website-pictures-Explosion-Bonding-opt.webp\u00bb alt=\u00bbPlaca revestida por explosi\u00f3n al vac\u00edo\u00bb title_text=\u00bbPlaca revestida por explosi\u00f3n al vac\u00edo\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb custom_margin=\u00bb||80px|||\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb-30px\u00bb box_shadow_vertical=\u00bb-30px\u00bb box_shadow_spread=\u00bb10px\u00bb global_colors_info=\u00bb{}\u00bb][\/et_pb_image][\/et_pb_column][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#FFFFFF\u00bb text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb link_font=\u00bb||||on|||#de8d02|\u00bb link_text_color=\u00bb#de8d02&#8243; ul_font=\u00bb||||||||\u00bb ul_line_height=\u00bb1.8em\u00bb header_2_font_size=\u00bb39px\u00bb header_3_font=\u00bbGoldman Sans|700|||||||\u00bb header_3_text_color=\u00bb#FFFFFF\u00bb header_3_font_size=\u00bb38px\u00bb header_3_line_height=\u00bb1.4em\u00bb custom_margin=\u00bb||-1px|||\u00bb custom_padding=\u00bb||0px|||\u00bb header_3_font_size_tablet=\u00bb\u00bb header_3_font_size_phone=\u00bb32px\u00bb header_3_font_size_last_edited=\u00bbon|phone\u00bb locked=\u00bboff\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><span style=\"color: #ffffff;\"><strong>Soldadura por explosi\u00f3n al vac\u00edo: control de proceso mejorado<\/strong><\/span><\/h2>\n<p>La <strong>soldadura por explosi\u00f3n al vac\u00edo<\/strong> es una variante avanzada del proceso convencional en la que la uni\u00f3n se realiza en un entorno de vac\u00edo controlado.<\/p>\n<p>Al eliminar el aire y reducir la oxidaci\u00f3n, el vac\u00edo mejora la limpieza de la interfaz y la calidad de la uni\u00f3n.<\/p>\n<p>El resultado:<\/p>\n<ul>\n<li>Mayor integridad metal\u00fargica<\/li>\n<li>Menor riesgo de contaminaci\u00f3n<\/li>\n<li>Mayor uniformidad del proceso<\/li>\n<li>Mejor rendimiento en aplicaciones cr\u00edticas<\/li>\n<li>Sin microfisuras en la interfaz de uni\u00f3n<\/li>\n<\/ul>\n<p>En Shockwave, la <a href=\"https:\/\/shockwave-clad.com\/es\/tecnologia\/\">soldadura por explosi\u00f3n al vac\u00edo<\/a> es nuestra especialidad y nos permite ofrecer soluciones de alta fiabilidad para sectores exigentes como la energ\u00eda, el offshore y el procesamiento qu\u00edmico.<\/p>\n<p>[\/et_pb_text][\/et_pb_column][\/et_pb_row][et_pb_row _builder_version=\u00bb4.16&#8243; module_alignment=\u00bbright\u00bb custom_padding=\u00bb30px|0px|0|0px|false|false\u00bb locked=\u00bboff\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb4_4&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_button button_url=\u00bb@ET-DC@eyJkeW5hbWljIjp0cnVlLCJjb250ZW50IjoicG9zdF9saW5rX3VybF9wYWdlIiwic2V0dGluZ3MiOnsicG9zdF9pZCI6IjE4In19@\u00bb button_text=\u00bbtodos los detalles del revestimiento por explosi\u00f3n al vac\u00edo\u00bb button_alignment=\u00bbright\u00bb _builder_version=\u00bb4.27.6&#8243; _dynamic_attributes=\u00bbbutton_url\u00bb custom_button=\u00bbon\u00bb button_text_size=\u00bb14px\u00bb button_bg_color=\u00bb#ffb356&#8243; button_border_color=\u00bb#000000&#8243; button_border_radius=\u00bb0px\u00bb button_letter_spacing=\u00bb3px\u00bb button_font=\u00bbGoldman Sans|700||on|||||\u00bb button_icon=\u00bb&#x24;||divi||400&#8243; button_on_hover=\u00bboff\u00bb background_layout=\u00bbdark\u00bb custom_margin=\u00bb|||\u00bb custom_padding=\u00bb30px|70px|30px|70px|true|false\u00bb animation_style=\u00bbfold\u00bb animation_direction=\u00bbright\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb-30px\u00bb box_shadow_vertical=\u00bb-30px\u00bb box_shadow_spread=\u00bb-10px\u00bb box_shadow_color=\u00bbrgba(255,179,86,0.4)\u00bb global_colors_info=\u00bb{}\u00bb button_text_size__hover_enabled=\u00bboff\u00bb button_one_text_size__hover_enabled=\u00bboff\u00bb button_two_text_size__hover_enabled=\u00bboff\u00bb button_text_color__hover_enabled=\u00bboff\u00bb button_one_text_color__hover_enabled=\u00bboff\u00bb button_two_text_color__hover_enabled=\u00bboff\u00bb button_border_width__hover_enabled=\u00bboff\u00bb button_one_border_width__hover_enabled=\u00bboff\u00bb button_two_border_width__hover_enabled=\u00bboff\u00bb button_border_color__hover_enabled=\u00bboff\u00bb button_one_border_color__hover_enabled=\u00bboff\u00bb button_two_border_color__hover_enabled=\u00bboff\u00bb button_border_radius__hover_enabled=\u00bboff\u00bb button_one_border_radius__hover_enabled=\u00bboff\u00bb button_two_border_radius__hover_enabled=\u00bboff\u00bb button_letter_spacing__hover_enabled=\u00bboff\u00bb button_one_letter_spacing__hover_enabled=\u00bboff\u00bb button_two_letter_spacing__hover_enabled=\u00bboff\u00bb button_bg_color__hover_enabled=\u00bboff\u00bb button_one_bg_color__hover_enabled=\u00bboff\u00bb button_two_bg_color__hover_enabled=\u00bboff\u00bb][\/et_pb_button][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.6&#8243; background_enable_color=\u00bboff\u00bb background_enable_image=\u00bboff\u00bb background_position=\u00bbtop_center\u00bb custom_padding=\u00bb54px|0px|0|0px|false|false\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row _builder_version=\u00bb4.27.4&#8243; custom_padding=\u00bb||0px||false|false\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb4_4&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#000000&#8243; text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb ul_text_color=\u00bb#000000&#8243; header_2_font_size=\u00bb39px\u00bb max_width=\u00bb1040px\u00bb custom_margin=\u00bb||||false|false\u00bb custom_margin_tablet=\u00bb|||0px\u00bb custom_margin_phone=\u00bb\u00bb custom_margin_last_edited=\u00bbon|desktop\u00bb custom_padding=\u00bb|0px||||\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><strong>Principales ventajas de la soldadura por explosi\u00f3n<\/strong><\/h2>\n<p><strong>Este proceso ofrece ventajas importantes<\/strong> frente a los m\u00e9todos de uni\u00f3n convencionales, especialmente en aplicaciones industriales de alto rendimiento y fiabilidad cr\u00edtica.<\/p>\n<p>Permite combinar metales que no pueden unirse mediante soldadura tradicional, abriendo nuevas posibilidades de dise\u00f1o.<\/p>\n<p>Al no haber fusi\u00f3n, se evita la distorsi\u00f3n t\u00e9rmica y se conservan las propiedades originales de ambos materiales. La uni\u00f3n resultante es extremadamente resistente y fiable en entornos exigentes.<\/p>\n<p>Otras ventajas:<\/p>\n<ul>\n<li>Excelente resistencia mec\u00e1nica<\/li>\n<li>Resistencia superior a la corrosi\u00f3n<\/li>\n<li>Coste inferior al de las aleaciones macizas<\/li>\n<li>Escalable a componentes de gran tama\u00f1o<\/li>\n<\/ul>\n<p>[\/et_pb_text][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.4&#8243; background_color=\u00bb#000000&#8243; background_image=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2025\/09\/electrician_19.png\u00bb background_position=\u00bbtop_center\u00bb min_height=\u00bb634.2px\u00bb custom_margin=\u00bb21px|||||\u00bb custom_padding=\u00bb54px|0px|0|0px|false|false\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row column_structure=\u00bb1_2,1_2&#8243; custom_padding_last_edited=\u00bbon|tablet\u00bb _builder_version=\u00bb4.27.4&#8243; custom_margin=\u00bb|auto|-28px|auto||\u00bb custom_padding=\u00bb||0px||false|false\u00bb custom_padding_tablet=\u00bb|||0px\u00bb custom_padding_phone=\u00bb\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_image src=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2026\/10\/Material-Combinations-1-opt.webp\u00bb alt=\u00bbEjemplo de combinaciones de materiales por soldadura por explosi\u00f3n\u00bb title_text=\u00bbEjemplo de combinaciones de materiales por soldadura por explosi\u00f3n\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb custom_margin=\u00bb||128px|||\u00bb custom_padding=\u00bb|6px|0px|||\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb-30px\u00bb box_shadow_vertical=\u00bb-30px\u00bb box_shadow_spread=\u00bb10px\u00bb global_colors_info=\u00bb{}\u00bb][\/et_pb_image][\/et_pb_column][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#FFFFFF\u00bb text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb ul_font=\u00bb||||||||\u00bb ul_line_height=\u00bb1.8em\u00bb header_2_font_size=\u00bb39px\u00bb header_3_font=\u00bbGoldman Sans|700|||||||\u00bb header_3_text_color=\u00bb#FFFFFF\u00bb header_3_font_size=\u00bb38px\u00bb header_3_line_height=\u00bb1.4em\u00bb header_3_font_size_tablet=\u00bb\u00bb header_3_font_size_phone=\u00bb32px\u00bb header_3_font_size_last_edited=\u00bbon|phone\u00bb locked=\u00bboff\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><span style=\"color: #ffffff;\"><strong>Combinaciones de materiales habituales<\/strong><\/span><\/h2>\n<p>Combinaciones t\u00edpicas:<\/p>\n<ul>\n<li>Aluminio con acero<\/li>\n<li>Titanio con acero inoxidable<\/li>\n<li>Cobre con aluminio<\/li>\n<li>Aleaciones de n\u00edquel con acero al carbono<\/li>\n<li>Acero inoxidable con acero al carbono<\/li>\n<li>Y muchas m\u00e1s<\/li>\n<\/ul>\n<p>Estas combinaciones son esenciales en aplicaciones que requieren a la vez resistencia mec\u00e1nica y resistencia a la corrosi\u00f3n, sobre todo en entornos industriales exigentes.<\/p>\n<p>En muchos casos no es posible lograrlas con t\u00e9cnicas de soldadura convencionales por las diferencias de punto de fusi\u00f3n, dilataci\u00f3n t\u00e9rmica y compatibilidad metal\u00fargica. Por ello, el revestimiento por explosi\u00f3n se ha convertido en una soluci\u00f3n clave en la ingenier\u00eda avanzada.<\/p>\n<p>[\/et_pb_text][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.6&#8243; da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row column_structure=\u00bb1_2,1_2&#8243; _builder_version=\u00bb4.27.4&#8243; custom_padding=\u00bb||0px||false|false\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#000000&#8243; text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb ul_text_color=\u00bb#000000&#8243; header_2_font_size=\u00bb39px\u00bb max_width=\u00bb600px\u00bb custom_margin=\u00bb||||false|false\u00bb custom_margin_tablet=\u00bb|||0px\u00bb custom_margin_phone=\u00bb\u00bb custom_margin_last_edited=\u00bbon|desktop\u00bb custom_padding=\u00bb||1px|||\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><strong>Principales aplicaciones industriales<\/strong><\/h2>\n<p><strong>La soldadura por explosi\u00f3n se utiliza<\/strong> en industrias donde los materiales deben trabajar en condiciones extremas y con una larga vida \u00fatil:<\/p>\n<ul>\n<li><strong>Petr\u00f3leo y gas: <\/strong>placas revestidas y juntas de transici\u00f3n para recipientes a presi\u00f3n, tuber\u00edas y equipos de proceso sometidos a alta presi\u00f3n y corrosi\u00f3n<\/li>\n<li><strong>Naval y offshore: <\/strong>juntas de transici\u00f3n estructurales como Triplate\u00ae aportan durabilidad y resistencia a la corrosi\u00f3n en ambientes marinos agresivos<\/li>\n<li><strong>Qu\u00edmica y petroqu\u00edmica: <\/strong>equipos dise\u00f1ados para soportar altas temperaturas y sustancias corrosivas<\/li>\n<li><strong>Generaci\u00f3n de energ\u00eda:<\/strong> componentes para intercambiadores de calor e infraestructuras cr\u00edticas que exigen alta fiabilidad<\/li>\n<li><strong>Transici\u00f3n energ\u00e9tica: <\/strong>cada vez m\u00e1s relevante en aplicaciones de hidr\u00f3geno, GNL y energ\u00edas renovables<\/li>\n<\/ul>\n<p><strong>Plantas desaladoras:<\/strong> placas revestidas resistentes a la corrosi\u00f3n para sistemas de desalaci\u00f3n de agua de mar, donde la resistencia a los cloruros es esencial.<\/p>\n<p>&nbsp;<\/p>\n<p>[\/et_pb_text][\/et_pb_column][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_image src=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2026\/10\/ChatGPT-Image-15-abr-2026-10_55_26-opt.webp\u00bb alt=\u00bbPrimera explosi\u00f3n al vac\u00edo para placas revestidas en Shockwave Metalworking Technologies\u00bb title_text=\u00bbPrimera explosi\u00f3n al vac\u00edo para placas revestidas en Shockwave\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb custom_margin=\u00bb30px|||||\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb30px\u00bb box_shadow_vertical=\u00bb30px\u00bb box_shadow_spread=\u00bb10px\u00bb global_colors_info=\u00bb{}\u00bb][\/et_pb_image][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.4&#8243; background_color=\u00bb#000000&#8243; background_image=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2025\/09\/electrician_19.png\u00bb background_position=\u00bbtop_center\u00bb custom_padding=\u00bb54px|0px|0|0px|false|false\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row custom_padding_last_edited=\u00bbon|tablet\u00bb _builder_version=\u00bb4.27.4&#8243; custom_margin=\u00bb|||\u00bb custom_padding=\u00bb||||false|false\u00bb custom_padding_tablet=\u00bb|||0px\u00bb custom_padding_phone=\u00bb\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb4_4&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#FFFFFF\u00bb text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb ul_font=\u00bb||||||||\u00bb ul_line_height=\u00bb1.8em\u00bb header_2_font_size=\u00bb39px\u00bb header_3_font=\u00bb|700|||||||\u00bb header_3_text_color=\u00bb#FFFFFF\u00bb header_3_font_size=\u00bb20px\u00bb header_3_line_height=\u00bb1.4em\u00bb header_3_font_size_tablet=\u00bb\u00bb header_3_font_size_phone=\u00bb32px\u00bb header_3_font_size_last_edited=\u00bbon|phone\u00bb locked=\u00bboff\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><span style=\"color: #ffffff;\"><strong>Soldadura por explosi\u00f3n frente a otros m\u00e9todos de uni\u00f3n<\/strong><\/span><\/h2>\n<p>Frente a m\u00e9todos tradicionales como la soldadura por fusi\u00f3n, la soldadura fuerte o el laminado, la soldadura por explosi\u00f3n ofrece ventajas \u00fanicas:<\/p>\n<p>&nbsp;<\/p>\n<table border=\"1\" style=\"width: 100%; border-collapse: collapse; border-style: solid;\">\n<tbody>\n<tr>\n<td style=\"width: 23.5772%; text-align: center;\">\n<h3>M\u00e9todo<\/h3>\n<\/td>\n<td style=\"width: 35.7723%; text-align: center;\">\n<h3>Limitaci\u00f3n<\/h3>\n<\/td>\n<td style=\"width: 40.6504%; text-align: center;\">\n<h3>Ventaja de la soldadura por explosi\u00f3n<\/h3>\n<\/td>\n<\/tr>\n<tr>\n<td style=\"text-align: center;\">Soldadura por fusi\u00f3n<\/td>\n<td style=\"text-align: center;\">Distorsi\u00f3n t\u00e9rmica<\/td>\n<td style=\"text-align: center;\">Sin fusi\u00f3n ni distorsi\u00f3n<\/td>\n<\/tr>\n<tr>\n<td style=\"text-align: center;\">Laminado (roll bonding)<\/td>\n<td style=\"text-align: center;\">Combinaciones de materiales limitadas<\/td>\n<td style=\"text-align: center;\">Amplia compatibilidad de materiales<\/td>\n<\/tr>\n<tr>\n<td style=\"text-align: center;\">Soldadura fuerte<\/td>\n<td style=\"text-align: center;\">Menor resistencia<\/td>\n<td style=\"text-align: center;\">Uni\u00f3n metal\u00fargica resistente<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p>[\/et_pb_text][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.6&#8243; background_enable_color=\u00bboff\u00bb background_enable_image=\u00bboff\u00bb background_position=\u00bbtop_center\u00bb custom_padding=\u00bb54px|0px|0|0px|false|false\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row column_structure=\u00bb1_2,1_2&#8243; _builder_version=\u00bb4.27.4&#8243; custom_padding=\u00bb||0px||false|false\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#000000&#8243; text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb link_font=\u00bb||||on|||#de8d02|\u00bb link_text_color=\u00bb#de8d02&#8243; ul_text_color=\u00bb#000000&#8243; header_2_font_size=\u00bb39px\u00bb max_width=\u00bb600px\u00bb custom_margin=\u00bb||-3px||false|false\u00bb custom_margin_tablet=\u00bb|||0px\u00bb custom_margin_phone=\u00bb\u00bb custom_margin_last_edited=\u00bbon|desktop\u00bb custom_padding=\u00bb||18px|||\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><strong>Productos y soluciones<\/strong><\/h2>\n<p>Este proceso permite fabricar componentes industriales de alto rendimiento para entornos exigentes:<\/p>\n<ul>\n<li><strong><a href=\"https:\/\/shockwave-clad.com\/es\/productos-placas-revestidas\/placas-revestidas\/\">Placas revestidas<\/a><\/strong>: placas compuestas que combinan materiales resistentes a la corrosi\u00f3n con resistencia estructural<\/li>\n<li><a href=\"https:\/\/shockwave-clad.com\/es\/juntas-transicion-metalicas\/\"><strong>Juntas de transici\u00f3n<\/strong><\/a><strong>: <\/strong>soluciones para unir metales dis\u00edmiles en tuber\u00edas y estructuras<\/li>\n<li><strong><a href=\"https:\/\/shockwave-clad.com\/es\/placas-tubulares\/\">Placas tubulares<\/a>:<\/strong> para intercambiadores de calor, con excelente resistencia mec\u00e1nica y a la corrosi\u00f3n<\/li>\n<\/ul>\n<p>Estos productos se utilizan ampliamente en industrias que requieren materiales de alto rendimiento y fiabilidad a largo plazo.<\/p>\n<p>[\/et_pb_text][\/et_pb_column][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_image src=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2026\/10\/Products-and-Solutions-opt.webp\u00bb alt=\u00bbEjemplo de producto obtenido por soldadura por explosi\u00f3n: una placa revestida\u00bb title_text=\u00bbEjemplo de producto obtenido por soldadura por explosi\u00f3n: una placa revestida\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb custom_margin=\u00bb-1px|||||\u00bb custom_padding=\u00bb||0px|||\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb30px\u00bb box_shadow_vertical=\u00bb30px\u00bb box_shadow_spread=\u00bb10px\u00bb global_colors_info=\u00bb{}\u00bb][\/et_pb_image][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.4&#8243; background_color=\u00bb#000000&#8243; background_image=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2025\/09\/electrician_19.png\u00bb background_position=\u00bbtop_center\u00bb custom_margin=\u00bb20px|||||\u00bb custom_padding=\u00bb0px|0px|0|0px|false|false\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row column_structure=\u00bb1_2,1_2&#8243; custom_padding_last_edited=\u00bbon|tablet\u00bb _builder_version=\u00bb4.27.4&#8243; custom_margin=\u00bb|||\u00bb custom_padding=\u00bb||35px||false|false\u00bb custom_padding_tablet=\u00bb|||0px\u00bb custom_padding_phone=\u00bb\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_image src=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2026\/10\/Joining-Dissimlar-Metals-opt.webp\u00bb alt=\u00bbCryoClad\u00ae, junta de transici\u00f3n criog\u00e9nica fabricada por soldadura por explosi\u00f3n en Shockwave\u00bb title_text=\u00bbCryoClad\u00ae, junta de transici\u00f3n criog\u00e9nica fabricada por soldadura por explosi\u00f3n en Shockwave\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb custom_margin=\u00bb30px|||||\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb30px\u00bb box_shadow_vertical=\u00bb30px\u00bb box_shadow_spread=\u00bb10px\u00bb global_colors_info=\u00bb{}\u00bb][\/et_pb_image][\/et_pb_column][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#FFFFFF\u00bb text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb link_font=\u00bb||||on|||#de8d02|\u00bb link_text_color=\u00bb#de8d02&#8243; ul_font=\u00bb||||||||\u00bb ul_line_height=\u00bb1.8em\u00bb header_2_font_size=\u00bb39px\u00bb header_3_font=\u00bbGoldman Sans|700|||||||\u00bb header_3_text_color=\u00bb#FFFFFF\u00bb header_3_font_size=\u00bb38px\u00bb header_3_line_height=\u00bb1.4em\u00bb hover_enabled=\u00bb0&#8243; header_3_font_size_tablet=\u00bb\u00bb header_3_font_size_phone=\u00bb32px\u00bb header_3_font_size_last_edited=\u00bbon|phone\u00bb locked=\u00bboff\u00bb global_colors_info=\u00bb{}\u00bb sticky_enabled=\u00bb0&#8243;]<\/p>\n<h2><span style=\"color: #ffffff;\"><strong>Uni\u00f3n de metales dis\u00edmiles<\/strong><\/span><\/h2>\n<p>Una de las principales ventajas de la soldadura por explosi\u00f3n es su capacidad para <a href=\"https:\/\/shockwave-clad.com\/joining-dissimilar-metals\/\">unir metales dis\u00edmiles<\/a> que son dif\u00edciles o imposibles de soldar con m\u00e9todos tradicionales, un reto importante en la ingenier\u00eda moderna.<\/p>\n<p>Nuestro proceso lo resuelve evitando la fusi\u00f3n y creando una uni\u00f3n metal\u00fargica directa entre los materiales.<\/p>\n<p>Por ejemplo:<\/p>\n<ul>\n<li>Aluminio con acero<\/li>\n<li>Cobre con aluminio<\/li>\n<li>Titanio con acero inoxidable<\/li>\n<\/ul>\n<p>Esta capacidad es esencial en industrias donde deben combinarse propiedades de materiales distintos.<\/p>\n<p>[\/et_pb_text][et_pb_button button_url=\u00bb@ET-DC@eyJkeW5hbWljIjp0cnVlLCJjb250ZW50IjoicG9zdF9saW5rX3VybF9wYWdlIiwic2V0dGluZ3MiOnsicG9zdF9pZCI6IjM0MjAifX0=@\u00bb button_text=\u00bbm\u00e1s informaci\u00f3n sobre la uni\u00f3n de metales dis\u00edmiles\u00bb button_alignment=\u00bbright\u00bb _builder_version=\u00bb4.27.6&#8243; _dynamic_attributes=\u00bbbutton_url\u00bb custom_button=\u00bbon\u00bb button_text_size=\u00bb14px\u00bb button_bg_color=\u00bb#ffb356&#8243; button_border_color=\u00bb#000000&#8243; button_border_radius=\u00bb0px\u00bb button_letter_spacing=\u00bb3px\u00bb button_font=\u00bbGoldman Sans|700||on|||||\u00bb button_icon=\u00bb&#x24;||divi||400&#8243; button_on_hover=\u00bboff\u00bb background_layout=\u00bbdark\u00bb custom_margin=\u00bb|-742px||||\u00bb custom_padding=\u00bb30px|70px|30px|70px|true|false\u00bb animation_style=\u00bbfold\u00bb animation_direction=\u00bbright\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb-30px\u00bb box_shadow_vertical=\u00bb-30px\u00bb box_shadow_spread=\u00bb-10px\u00bb box_shadow_color=\u00bbrgba(255,179,86,0.4)\u00bb global_colors_info=\u00bb{}\u00bb button_text_size__hover_enabled=\u00bboff\u00bb button_one_text_size__hover_enabled=\u00bboff\u00bb button_two_text_size__hover_enabled=\u00bboff\u00bb button_text_color__hover_enabled=\u00bboff\u00bb button_one_text_color__hover_enabled=\u00bboff\u00bb button_two_text_color__hover_enabled=\u00bboff\u00bb button_border_width__hover_enabled=\u00bboff\u00bb button_one_border_width__hover_enabled=\u00bboff\u00bb button_two_border_width__hover_enabled=\u00bboff\u00bb button_border_color__hover_enabled=\u00bboff\u00bb button_one_border_color__hover_enabled=\u00bboff\u00bb button_two_border_color__hover_enabled=\u00bboff\u00bb button_border_radius__hover_enabled=\u00bboff\u00bb button_one_border_radius__hover_enabled=\u00bboff\u00bb button_two_border_radius__hover_enabled=\u00bboff\u00bb button_letter_spacing__hover_enabled=\u00bboff\u00bb button_one_letter_spacing__hover_enabled=\u00bboff\u00bb button_two_letter_spacing__hover_enabled=\u00bboff\u00bb button_bg_color__hover_enabled=\u00bboff\u00bb button_one_bg_color__hover_enabled=\u00bboff\u00bb button_two_bg_color__hover_enabled=\u00bboff\u00bb][\/et_pb_button][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.6&#8243; background_enable_color=\u00bboff\u00bb background_enable_image=\u00bboff\u00bb background_position=\u00bbtop_center\u00bb custom_margin=\u00bb-34px|||||\u00bb custom_padding=\u00bb54px|0px|0|0px|false|false\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row column_structure=\u00bb1_2,1_2&#8243; _builder_version=\u00bb4.27.4&#8243; custom_padding=\u00bb||0px||false|false\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; text_font=\u00bb||||||||\u00bb text_text_color=\u00bb#000000&#8243; text_font_size=\u00bb16px\u00bb text_line_height=\u00bb1.8em\u00bb link_font=\u00bb||||on|||#de8d02|\u00bb link_text_color=\u00bb#de8d02&#8243; ul_text_color=\u00bb#000000&#8243; header_2_font_size=\u00bb39px\u00bb max_width=\u00bb600px\u00bb custom_margin=\u00bb||||false|false\u00bb custom_margin_tablet=\u00bb|||0px\u00bb custom_margin_phone=\u00bb\u00bb custom_margin_last_edited=\u00bbon|desktop\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><strong>Por qu\u00e9 elegir Shockwave para la soldadura por explosi\u00f3n<\/strong><\/h2>\n<p>En Shockwave estamos especializados en la <strong>tecnolog\u00eda de soldadura por explosi\u00f3n al vac\u00edo<\/strong>, garantizando resultados de alta calidad para aplicaciones industriales exigentes.<\/p>\n<p>Nuestras capacidades:<\/p>\n<ul>\n<li>Control avanzado del proceso y experiencia en ingenier\u00eda<\/li>\n<li>Calidad de fabricaci\u00f3n constante<\/li>\n<li>Soluciones a medida para requisitos complejos<\/li>\n<li>Experiencia en industrias de alto rendimiento<\/li>\n<\/ul>\n<p>Nuestro <strong>proceso en vac\u00edo ofrece un control superior<\/strong> frente al proceso convencional, con interfaces m\u00e1s limpias, mayor uniformidad y m\u00e1s fiabilidad en aplicaciones cr\u00edticas.<\/p>\n<p>[\/et_pb_text][et_pb_text _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb custom_margin=\u00bb|-578px||||\u00bb custom_padding=\u00bb|||0px||\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><strong>\u00bfBusca soluciones de soldadura por explosi\u00f3n?<\/strong><\/h2>\n<p>Contacte con nuestro equipo para analizar los requisitos de su proyecto y descubrir c\u00f3mo Shockwave puede ofrecerle soluciones fiables de soldadura por explosi\u00f3n.<\/p>\n<p>[\/et_pb_text][\/et_pb_column][et_pb_column type=\u00bb1_2&#8243; _builder_version=\u00bb4.16&#8243; custom_padding=\u00bb|||\u00bb global_colors_info=\u00bb{}\u00bb custom_padding__hover=\u00bb|||\u00bb][et_pb_image src=\u00bbhttps:\/\/shockwave-clad.com\/wp-content\/uploads\/2026\/10\/Why-Choose-Shockwave-opt.webp\u00bb alt=\u00bbInstalaciones de Shockwave Metalworking Technologies donde se realiza la soldadura por explosi\u00f3n al vac\u00edo\u00bb title_text=\u00bbInstalaciones de Shockwave Metalworking Technologies donde se realiza la soldadura por explosi\u00f3n al vac\u00edo\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb custom_margin=\u00bb30px|||||\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb30px\u00bb box_shadow_vertical=\u00bb30px\u00bb box_shadow_spread=\u00bb10px\u00bb global_colors_info=\u00bb{}\u00bb][\/et_pb_image][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; admin_label=\u00bbAbout Us\u00bb _builder_version=\u00bb4.27.6&#8243; background_enable_color=\u00bboff\u00bb background_enable_image=\u00bboff\u00bb background_position=\u00bbtop_center\u00bb custom_padding=\u00bb54px|0px|0|0px|false|false\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb custom_margin=\u00bb|2px||auto||\u00bb custom_padding=\u00bb0px|||||\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb4_4&#8243; _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_button button_url=\u00bb@ET-DC@eyJkeW5hbWljIjp0cnVlLCJjb250ZW50IjoicG9zdF9saW5rX3VybF9wYWdlIiwic2V0dGluZ3MiOnsicG9zdF9pZCI6IjIwIn19@\u00bb button_text=\u00bbSOLICITAR PRESUPUESTO\u00bb button_alignment=\u00bbright\u00bb _builder_version=\u00bb4.27.6&#8243; _dynamic_attributes=\u00bbbutton_url\u00bb custom_button=\u00bbon\u00bb button_text_size=\u00bb14px\u00bb button_bg_color=\u00bb#ffb356&#8243; button_border_color=\u00bb#000000&#8243; button_border_radius=\u00bb0px\u00bb button_letter_spacing=\u00bb3px\u00bb button_font=\u00bbGoldman Sans|700||on|||||\u00bb button_icon=\u00bb&#x24;||divi||400&#8243; button_on_hover=\u00bboff\u00bb background_layout=\u00bbdark\u00bb custom_margin=\u00bb||-15px|||\u00bb custom_padding=\u00bb30px|70px|30px|70px|true|false\u00bb animation_style=\u00bbfold\u00bb animation_direction=\u00bbright\u00bb box_shadow_style=\u00bbpreset4&#8243; box_shadow_horizontal=\u00bb-30px\u00bb box_shadow_vertical=\u00bb-30px\u00bb box_shadow_spread=\u00bb-10px\u00bb box_shadow_color=\u00bbrgba(255,179,86,0.4)\u00bb global_colors_info=\u00bb{}\u00bb button_text_size__hover_enabled=\u00bboff\u00bb button_one_text_size__hover_enabled=\u00bboff\u00bb button_two_text_size__hover_enabled=\u00bboff\u00bb button_text_color__hover_enabled=\u00bboff\u00bb button_one_text_color__hover_enabled=\u00bboff\u00bb button_two_text_color__hover_enabled=\u00bboff\u00bb button_border_width__hover_enabled=\u00bboff\u00bb button_one_border_width__hover_enabled=\u00bboff\u00bb button_two_border_width__hover_enabled=\u00bboff\u00bb button_border_color__hover_enabled=\u00bboff\u00bb button_one_border_color__hover_enabled=\u00bboff\u00bb button_two_border_color__hover_enabled=\u00bboff\u00bb button_border_radius__hover_enabled=\u00bboff\u00bb button_one_border_radius__hover_enabled=\u00bboff\u00bb button_two_border_radius__hover_enabled=\u00bboff\u00bb button_letter_spacing__hover_enabled=\u00bboff\u00bb button_one_letter_spacing__hover_enabled=\u00bboff\u00bb button_two_letter_spacing__hover_enabled=\u00bboff\u00bb button_bg_color__hover_enabled=\u00bboff\u00bb button_one_bg_color__hover_enabled=\u00bboff\u00bb button_two_bg_color__hover_enabled=\u00bboff\u00bb][\/et_pb_button][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb background_color=\u00bb#000000&#8243; min_height=\u00bb706.5px\u00bb custom_padding=\u00bb33px|||||\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_row _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb background_color=\u00bb#000000&#8243; global_colors_info=\u00bb{}\u00bb][et_pb_column type=\u00bb4_4&#8243; _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb global_colors_info=\u00bb{}\u00bb][et_pb_text _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb custom_margin=\u00bb-7px|||||\u00bb custom_padding=\u00bb16px|||||\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<h2><span style=\"color: #ffffff;\"><strong>Preguntas frecuentes sobre la soldadura por explosi\u00f3n<\/strong><\/span><\/h2>\n<p>[\/et_pb_text][et_pb_accordion open_toggle_text_color=\u00bb#000000&#8243; closed_toggle_background_color=\u00bb#000000&#8243; toggle_icon=\u00bb&#x3a;||divi||400&#8243; _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb toggle_text_color=\u00bb#FFFFFF\u00bb toggle_level=\u00bbh3&#8243; toggle_font_size=\u00bb20px\u00bb background_color=\u00bb#000000&#8243; global_colors_info=\u00bb{}\u00bb][et_pb_accordion_item title=\u00bb\u00bfPara qu\u00e9 se utiliza la soldadura por explosi\u00f3n?\u00bb open=\u00bbon\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb global_colors_info=\u00bb{}\u00bb]<\/p>\n<p><span style=\"color: #000000;\">Para unir metales dis\u00edmiles en aplicaciones industriales que requieren alta resistencia y resistencia a la corrosi\u00f3n.<\/span><\/p>\n<p>[\/et_pb_accordion_item][et_pb_accordion_item title=\u00bb\u00bfEs la soldadura por explosi\u00f3n mejor que la soldadura convencional?\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb global_colors_info=\u00bb{}\u00bb open=\u00bboff\u00bb]<\/p>\n<p>Con metales dis\u00edmiles suele ofrecer mejores resultados que la soldadura tradicional, porque evita la fusi\u00f3n y conserva las propiedades de los materiales.<\/p>\n<p>[\/et_pb_accordion_item][et_pb_accordion_item title=\u00bb\u00bfQu\u00e9 diferencia hay entre explosion bonding, explosion welding y explosion cladding?\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb global_colors_info=\u00bb{}\u00bb open=\u00bboff\u00bb]<\/p>\n<p>Los tres t\u00e9rminos se refieren al mismo proceso; \u00abexplosion bonding\u00bb es el m\u00e1s utilizado en el \u00e1mbito industrial.<\/p>\n<p>[\/et_pb_accordion_item][et_pb_accordion_item title=\u00bb\u00bfQu\u00e9 materiales se pueden unir con este proceso?\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb global_colors_info=\u00bb{}\u00bb open=\u00bboff\u00bb]<\/p>\n<p>Se puede combinar una amplia gama de metales, como aluminio, acero, titanio, cobre y acero inoxidable.<\/p>\n<p>[\/et_pb_accordion_item][et_pb_accordion_item title=\u00bb\u00bfEn qu\u00e9 se diferencia de la soldadura tradicional?\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb global_colors_info=\u00bb{}\u00bb open=\u00bboff\u00bb]<\/p>\n<p>La soldadura por explosi\u00f3n une los metales sin fundirlos, mediante un impacto a alta velocidad generado por energ\u00eda explosiva controlada. La soldadura tradicional funde los materiales con calor, lo que puede causar distorsi\u00f3n y limita la uni\u00f3n de metales dis\u00edmiles.<\/p>\n<p>Al ser un proceso en estado s\u00f3lido, conserva las propiedades de los materiales y es m\u00e1s adecuado para aplicaciones de alto rendimiento.<\/p>\n<p>[\/et_pb_accordion_item][et_pb_accordion_item title=\u00bb\u00bfPor qu\u00e9 es importante en la industria?\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb global_colors_info=\u00bb{}\u00bb open=\u00bboff\u00bb]<\/p>\n<p>Permite a los ingenieros combinar materiales con propiedades diferentes, mejorando el rendimiento y prolongando la vida \u00fatil de los componentes.<\/p>\n<p>[\/et_pb_accordion_item][\/et_pb_accordion][\/et_pb_column][\/et_pb_row][\/et_pb_section][et_pb_section fb_built=\u00bb1&#8243; fullwidth=\u00bbon\u00bb _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb da_disable_devices=\u00bboff|off|off\u00bb global_colors_info=\u00bb{}\u00bb da_is_popup=\u00bboff\u00bb da_exit_intent=\u00bboff\u00bb da_has_close=\u00bbon\u00bb da_alt_close=\u00bboff\u00bb da_dark_close=\u00bboff\u00bb da_not_modal=\u00bbon\u00bb da_is_singular=\u00bboff\u00bb da_with_loader=\u00bboff\u00bb da_has_shadow=\u00bbon\u00bb][et_pb_fullwidth_code _builder_version=\u00bb4.27.6&#8243; _module_preset=\u00bbdefault\u00bb global_colors_info=\u00bb{}\u00bb]<script type=\"application\/ld+json\">{\"@context\":\"https:\/\/schema.org\",\"@type\":\"FAQPage\",\"mainEntity\":[{\"@type\":\"Question\",\"name\":\"\u00bfQu\u00e9 es la soldadura por explosi\u00f3n?\",\"acceptedAnswer\":{\"@type\":\"Answer\",\"text\":\"Es un proceso de soldadura en estado s\u00f3lido que une metales dis\u00edmiles sin fundirlos, utilizando energ\u00eda explosiva controlada para crear una uni\u00f3n metal\u00fargica resistente.\"}},{\"@type\":\"Question\",\"name\":\"\u00bfPara qu\u00e9 se utiliza la soldadura por explosi\u00f3n?\",\"acceptedAnswer\":{\"@type\":\"Answer\",\"text\":\"Para fabricar placas revestidas, juntas de transici\u00f3n y otros componentes que requieren alta resistencia y resistencia a la corrosi\u00f3n en sectores como el petr\u00f3leo y gas, la energ\u00eda y la industria qu\u00edmica.\"}},{\"@type\":\"Question\",\"name\":\"\u00bfC\u00f3mo funciona la soldadura por explosi\u00f3n?\",\"acceptedAnswer\":{\"@type\":\"Answer\",\"text\":\"Se detona una carga explosiva que proyecta un metal contra otro a gran velocidad. El impacto crea una uni\u00f3n metal\u00fargica por deformaci\u00f3n pl\u00e1stica en la interfaz.\"}},{\"@type\":\"Question\",\"name\":\"\u00bfQu\u00e9 materiales se pueden unir?\",\"acceptedAnswer\":{\"@type\":\"Answer\",\"text\":\"Una amplia gama de metales dis\u00edmiles: aluminio con acero, titanio con acero inoxidable, cobre con aluminio y aleaciones de n\u00edquel con acero al carbono, entre otros.\"}},{\"@type\":\"Question\",\"name\":\"\u00bfEs mejor que la soldadura convencional?\",\"acceptedAnswer\":{\"@type\":\"Answer\",\"text\":\"Para metales dis\u00edmiles suele preferirse porque no funde los materiales, conserva sus propiedades y evita la distorsi\u00f3n y la incompatibilidad metal\u00fargica.\"}}]}<\/script>[\/et_pb_fullwidth_code][\/et_pb_section]<\/p>\n","protected":false},"excerpt":{"rendered":"<p>Soldadura por explosi\u00f3n: proceso, aplicaciones y ventajasLa soldadura por explosi\u00f3n (explosion bonding) es un proceso de soldadura en fr\u00edo por presi\u00f3n en estado s\u00f3lido que une metales dis\u00edmiles sin fundirlos. Mediante energ\u00eda explosiva controlada, esta t\u00e9cnica crea una uni\u00f3n at\u00f3mica de alta resistencia entre materiales con propiedades muy diferentes. Esto permite fabricar placas revestidas (clad [&hellip;]<\/p>\n","protected":false},"author":3,"featured_media":0,"parent":0,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_et_pb_use_builder":"on","_et_pb_old_content":"","_et_gb_content_width":"","footnotes":""},"class_list":["post-4184","page","type-page","status-publish","hentry"],"yoast_head":"<!-- This site is optimized with the Yoast SEO plugin v28.7 - https:\/\/yoast.com\/product\/yoast-seo-wordpress\/ -->\n<title>Soldadura por explosi\u00f3n: proceso y aplicaciones | Shockwave<\/title>\n<meta name=\"description\" content=\"Qu\u00e9 es la soldadura por explosi\u00f3n (explosion bonding), c\u00f3mo funciona, ventajas, combinaciones de metales y aplicaciones industriales. Especialistas en vac\u00edo desde 1985.\" \/>\n<meta name=\"robots\" content=\"index, follow, max-snippet:-1, max-image-preview:large, max-video-preview:-1\" \/>\n<link rel=\"canonical\" href=\"https:\/\/shockwave-clad.com\/es\/soldadura-por-explosion\/\" \/>\n<meta property=\"og:locale\" content=\"es_ES\" \/>\n<meta property=\"og:type\" content=\"article\" \/>\n<meta property=\"og:title\" content=\"Soldadura por explosi\u00f3n: proceso y aplicaciones | Shockwave\" \/>\n<meta property=\"og:description\" content=\"Qu\u00e9 es la soldadura por explosi\u00f3n (explosion bonding), c\u00f3mo funciona, ventajas, combinaciones de metales y aplicaciones industriales. Especialistas en vac\u00edo desde 1985.\" \/>\n<meta property=\"og:url\" content=\"https:\/\/shockwave-clad.com\/es\/soldadura-por-explosion\/\" \/>\n<meta property=\"og:site_name\" content=\"Shockwave\" \/>\n<meta property=\"article:modified_time\" content=\"2026-10-22T11:39:00+00:00\" \/>\n<meta property=\"og:image\" content=\"https:\/\/shockwave-clad.com\/wp-content\/uploads\/2025\/12\/bc9ce71b-e94a-4f74-8aef-8218cb8ed95b.jpg\" \/>\n\t<meta property=\"og:image:width\" content=\"2048\" \/>\n\t<meta property=\"og:image:height\" content=\"1536\" \/>\n\t<meta property=\"og:image:type\" content=\"image\/jpeg\" \/>\n<meta name=\"twitter:card\" content=\"summary_large_image\" \/>\n<meta name=\"twitter:label1\" content=\"Tiempo de lectura\" \/>\n\t<meta name=\"twitter:data1\" content=\"31 minutos\" \/>\n<script type=\"application\/ld+json\" class=\"yoast-schema-graph\">{\"@context\":\"https:\\\/\\\/schema.org\",\"@graph\":[{\"@type\":\"WebPage\",\"@id\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/soldadura-por-explosion\\\/\",\"url\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/soldadura-por-explosion\\\/\",\"name\":\"Soldadura por explosi\u00f3n: proceso y aplicaciones | Shockwave\",\"isPartOf\":{\"@id\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/#website\"},\"datePublished\":\"2026-04-16T06:27:58+00:00\",\"dateModified\":\"2026-10-22T11:39:00+00:00\",\"description\":\"Qu\u00e9 es la soldadura por explosi\u00f3n (explosion bonding), c\u00f3mo funciona, ventajas, combinaciones de metales y aplicaciones industriales. Especialistas en vac\u00edo desde 1985.\",\"breadcrumb\":{\"@id\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/soldadura-por-explosion\\\/#breadcrumb\"},\"inLanguage\":\"es\",\"potentialAction\":[{\"@type\":\"ReadAction\",\"target\":[\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/soldadura-por-explosion\\\/\"]}]},{\"@type\":\"BreadcrumbList\",\"@id\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/soldadura-por-explosion\\\/#breadcrumb\",\"itemListElement\":[{\"@type\":\"ListItem\",\"position\":1,\"name\":\"Home\",\"item\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/\"},{\"@type\":\"ListItem\",\"position\":2,\"name\":\"Soldadura por explosi\u00f3n\"}]},{\"@type\":\"WebSite\",\"@id\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/#website\",\"url\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/\",\"name\":\"Shockwave\",\"description\":\"Shockwave Metalworking Technologies\",\"publisher\":{\"@id\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/#organization\"},\"alternateName\":\"Shockwave Metalworking Technologies\",\"potentialAction\":[{\"@type\":\"SearchAction\",\"target\":{\"@type\":\"EntryPoint\",\"urlTemplate\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/?s={search_term_string}\"},\"query-input\":{\"@type\":\"PropertyValueSpecification\",\"valueRequired\":true,\"valueName\":\"search_term_string\"}}],\"inLanguage\":\"es\"},{\"@type\":\"Organization\",\"@id\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/#organization\",\"name\":\"Shockwave Metalworking Technologies BV\",\"alternateName\":\"Shockwave\",\"url\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/\",\"logo\":{\"@type\":\"ImageObject\",\"inLanguage\":\"es\",\"@id\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/#\\\/schema\\\/logo\\\/image\\\/\",\"url\":\"https:\\\/\\\/shockwave-clad.com\\\/wp-content\\\/uploads\\\/2025\\\/09\\\/logo-shockwave.png\",\"contentUrl\":\"https:\\\/\\\/shockwave-clad.com\\\/wp-content\\\/uploads\\\/2025\\\/09\\\/logo-shockwave.png\",\"width\":300,\"height\":343,\"caption\":\"Shockwave Metalworking Technologies BV\"},\"image\":{\"@id\":\"https:\\\/\\\/shockwave-clad.com\\\/es\\\/#\\\/schema\\\/logo\\\/image\\\/\"},\"sameAs\":[\"https:\\\/\\\/www.linkedin.com\\\/company\\\/shockwave-metalworking-technologies-b-v\\\/\"]}]}<\/script>\n<!-- \/ Yoast SEO plugin. -->","yoast_head_json":{"title":"Soldadura por explosi\u00f3n: proceso y aplicaciones | Shockwave","description":"Qu\u00e9 es la soldadura por explosi\u00f3n (explosion bonding), c\u00f3mo funciona, ventajas, combinaciones de metales y aplicaciones industriales. Especialistas en vac\u00edo desde 1985.","robots":{"index":"index","follow":"follow","max-snippet":"max-snippet:-1","max-image-preview":"max-image-preview:large","max-video-preview":"max-video-preview:-1"},"canonical":"https:\/\/shockwave-clad.com\/es\/soldadura-por-explosion\/","og_locale":"es_ES","og_type":"article","og_title":"Soldadura por explosi\u00f3n: proceso y aplicaciones | Shockwave","og_description":"Qu\u00e9 es la soldadura por explosi\u00f3n (explosion bonding), c\u00f3mo funciona, ventajas, combinaciones de metales y aplicaciones industriales. Especialistas en vac\u00edo desde 1985.","og_url":"https:\/\/shockwave-clad.com\/es\/soldadura-por-explosion\/","og_site_name":"Shockwave","article_modified_time":"2026-10-22T11:39:00+00:00","og_image":[{"width":2048,"height":1536,"url":"https:\/\/shockwave-clad.com\/wp-content\/uploads\/2025\/12\/bc9ce71b-e94a-4f74-8aef-8218cb8ed95b.jpg","type":"image\/jpeg"}],"twitter_card":"summary_large_image","twitter_misc":{"Tiempo de lectura":"31 minutos"},"schema":{"@context":"https:\/\/schema.org","@graph":[{"@type":"WebPage","@id":"https:\/\/shockwave-clad.com\/es\/soldadura-por-explosion\/","url":"https:\/\/shockwave-clad.com\/es\/soldadura-por-explosion\/","name":"Soldadura por explosi\u00f3n: proceso y aplicaciones | Shockwave","isPartOf":{"@id":"https:\/\/shockwave-clad.com\/es\/#website"},"datePublished":"2026-04-16T06:27:58+00:00","dateModified":"2026-10-22T11:39:00+00:00","description":"Qu\u00e9 es la soldadura por explosi\u00f3n (explosion bonding), c\u00f3mo funciona, ventajas, combinaciones de metales y aplicaciones industriales. Especialistas en vac\u00edo desde 1985.","breadcrumb":{"@id":"https:\/\/shockwave-clad.com\/es\/soldadura-por-explosion\/#breadcrumb"},"inLanguage":"es","potentialAction":[{"@type":"ReadAction","target":["https:\/\/shockwave-clad.com\/es\/soldadura-por-explosion\/"]}]},{"@type":"BreadcrumbList","@id":"https:\/\/shockwave-clad.com\/es\/soldadura-por-explosion\/#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"Home","item":"https:\/\/shockwave-clad.com\/es\/"},{"@type":"ListItem","position":2,"name":"Soldadura por explosi\u00f3n"}]},{"@type":"WebSite","@id":"https:\/\/shockwave-clad.com\/es\/#website","url":"https:\/\/shockwave-clad.com\/es\/","name":"Shockwave","description":"Shockwave Metalworking Technologies","publisher":{"@id":"https:\/\/shockwave-clad.com\/es\/#organization"},"alternateName":"Shockwave Metalworking Technologies","potentialAction":[{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https:\/\/shockwave-clad.com\/es\/?s={search_term_string}"},"query-input":{"@type":"PropertyValueSpecification","valueRequired":true,"valueName":"search_term_string"}}],"inLanguage":"es"},{"@type":"Organization","@id":"https:\/\/shockwave-clad.com\/es\/#organization","name":"Shockwave Metalworking Technologies BV","alternateName":"Shockwave","url":"https:\/\/shockwave-clad.com\/es\/","logo":{"@type":"ImageObject","inLanguage":"es","@id":"https:\/\/shockwave-clad.com\/es\/#\/schema\/logo\/image\/","url":"https:\/\/shockwave-clad.com\/wp-content\/uploads\/2025\/09\/logo-shockwave.png","contentUrl":"https:\/\/shockwave-clad.com\/wp-content\/uploads\/2025\/09\/logo-shockwave.png","width":300,"height":343,"caption":"Shockwave Metalworking Technologies BV"},"image":{"@id":"https:\/\/shockwave-clad.com\/es\/#\/schema\/logo\/image\/"},"sameAs":["https:\/\/www.linkedin.com\/company\/shockwave-metalworking-technologies-b-v\/"]}]}},"_hostinger_reach_plugin_has_subscription_block":false,"_hostinger_reach_plugin_is_elementor":false,"_links":{"self":[{"href":"https:\/\/shockwave-clad.com\/es\/wp-json\/wp\/v2\/pages\/4184","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/shockwave-clad.com\/es\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/shockwave-clad.com\/es\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/shockwave-clad.com\/es\/wp-json\/wp\/v2\/users\/3"}],"replies":[{"embeddable":true,"href":"https:\/\/shockwave-clad.com\/es\/wp-json\/wp\/v2\/comments?post=4184"}],"version-history":[{"count":2,"href":"https:\/\/shockwave-clad.com\/es\/wp-json\/wp\/v2\/pages\/4184\/revisions"}],"predecessor-version":[{"id":4462,"href":"https:\/\/shockwave-clad.com\/es\/wp-json\/wp\/v2\/pages\/4184\/revisions\/4462"}],"wp:attachment":[{"href":"https:\/\/shockwave-clad.com\/es\/wp-json\/wp\/v2\/media?parent=4184"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}